Investigation of the Causes of Thermal Run-away in Sealed Nickel-Cadmium Batteries

It is shown from analysis of charging current and voltage change on the terminals of sealed Ni-Cd battery at thermal runaway, that thermal runaway is accompanied by a new high-power electrochemical reaction, going at battery voltage of approximately 0.55 V.